® - (Nylon 6/6 Extruded)
PROPERTY UNITS ASTM TEST NATURAL MoS2 FILLED
Density gm/cm3 D792 1.15 1.15
Tensile Strength at Yield 73ºF psi D638 11.800 11.800
Tensile Modulus of Elasticity 73ºF psi D638 450.000 450.000
Elongation 73oF % D638 20 - 60 20 - 60
Flexural Modulus of Elasticity 73ºF psi D790 365.500 365.500
Flexural Strength 73ºF psi D790 14.500 14.500
Shear Strength 73ºF psi D732 9.500 9.500
Coefficient of Friction 73ºF - - 0.35 - 0.45 0.35 - 0.45
IZOD Impact Strength 73ºF ft-lbs/inch D256 2.5 2.5
Hardness 73ºF - D785 R115 R115
Tensile Impact ft-lbs/inch D1822 90 - 170 90 - 170
Deformation Under Load % D621 1, 0 - 3, 0 1, 0 - 3, 0
Melting Point oF D789 491 491
Coefficient of Linear Thermal Expansion 1/K D696 4.5 x 10-5 4.5 x 10-5
Continuous Service Temperature in Air (Max) ºF - 248 248
Deflection Temperature 66 psi ºF D648 430 430
Deflection Temperature 264 psi ºF D648 200 - 450 200 - 450
Flammability - According to UL 94 (1) * UL 94 V - 2 V - 2
Flammability - According to ASTM (2) % D2863 26 26
Comparitive Tracking Index - D3638 CTI 600 CTI 600
Volume Resistivity Ohm/cm D257 1014 1014
Dielectric Constant (103 Hz) - D150 3.6 3.6
Dielectric Constant (10 x Hz) - D150 3.4 3.4
Dissipation Factor (Tan :- at 103 Hz) - D150 0.015 0.015
Dielectric Strength KV/mm D149 > 12 > 12
 

Sustamid 6/6 - Nylon 6/6 - is a tough, wear resistant formulation that performs well even at very low temperatures. It offers good damping capacities and high compressive strength.

 